Influence of the solubility of soy protein isolate on the mechanical properties of heat-set gels

Favoritar este trabalho
Como citar esse trabalho?
Detalhes
  • Tipo de apresentação: Pôster
  • Eixo temático: Engenharia de Processos e Tecnologias Emergentes (ET)
  • Palavras chaves: Emulsion-filled gels; soy protein isolate; gel structure;
  • 1 Faculdade de Zootecnia e Engenharia de Alimentos (FZEA/USP)

Influence of the solubility of soy protein isolate on the mechanical properties of heat-set gels

Letícia dos Santos Ferreira

Universidade Federal da Paraíba

Resumo

The low solubility of soy protein isolates (SPI) available in the market can be a technological challenge in their utilization for gelation. It is possible to increase the SPI solubility before gelation, and this study aimed to be a contribution in this area. Before gel production, the SPI dispersions were pre-processed by mechanical stirring, at room temperature, at different operational conditions - 400, 600 and 800 rpm, for 10, 20 and 30 min. The stirring was performed using a naval propeller. SPI (11, 13 and 15 g protein/100 g) heat-set gels (95 ⸰C, 30 min) were then produced and characterized in terms of morphology and uniaxial compression. In addition, the gels were produced as non-filled (NFG) and emulsion-filled gels (EFG). EFG were loaded with Brazil nut oil emulsion, stabilized with SPI as surfactant (5 g oil/100 g emulsion; 1 g/100 g SPI as surfactant). The pre-processing by mechanical stirring had a strong influence on the solubility of SPI; the higher the SPI concentration, the higher the solubility of SPI. By microscopy, the morphology of the gels was observed, and they were formed by large and dense aggregates resembling microgels. These microgels were apparently formed by smaller aggregates of soy proteins, also distinguishable in the micrographs. As for EFG, the oil droplets apparently interacted both among them and with the protein network, and they were preferentially located in the gel pores. The incorporation of oil droplets in the gel caused a remarkable increase in the Young´s modulus and rupture tension of the SPI gels, indicating the droplets were active particles. However, the increase in the solubility of SPI (30 to 60%) was not enough, apparently, to influence significantly on the values of mechanical properties of either NGF or EFG.

Compartilhe suas ideias ou dúvidas com os autores!

Sabia que o maior estímulo no desenvolvimento científico e cultural é a curiosidade? Deixe seus questionamentos ou sugestões para o autor!

Faça login para interagir

Tem uma dúvida ou sugestão? Compartilhe seu feedback com os autores!