MECHANICAL PROPERTIES OF GELATIN FILMS CONTAINING CELLULOSE NANOFIBER FROM SOYBEAN STRAW

Vol 2, 2022 - 153796
Pôster
Favorite this paper
How to cite this paper?
Abstract

Cellulose nanofibers (CNF) are appealing candidates for reinforcing biodegradable films. Nevertheless, the knowledge about the physical properties of films containing CNF is still very limited when compared with cellulose nanocrystal. The objective of this study was to evaluate the effect of cellulose nanofiber concentration on the mechanical properties of films based on type A and B gelatin. Soybean straw was chemically treated with a 17.5% NaOH solution (w/v)/15h and bleached using a 4% solution H2O2, 0.3% MgSO4.7H2O and 2% NaOH (w/v) at 90°C/3h. CNF extraction was performed by enzymatic hydrolysis of 3 g soybean straw/150 mL of sodium acetate buffer with 280 μL of an enzyme cocktail Optimash™ VR (DuPont Inc, USA) at pH 4.0 and 50°C/42h, followed by mechanical treatment (15000 rpm/5min) and sonication (70% amplitude/3 min).The films were prepared by casting technique with 4 g of gelatin/100 g of film forming solution and 0, 1, 3, 5 of CNF/100 g of gelatin, using 30 g glycerol/100 g gelatin. The mechanical properties were determined by uniaxial tensile tests (ASTM method D882-10), using a texturometer (TAXT2, TA Instruments, USA). The tensile strength (TS), elongation at break (E) and elastic modulus (M), were determined. Film thickness was measured using a digital micrometer (Absolute ID-C112B, Mitutoyo, Japan). The film thickness was approximately 85 µm, and not significantly affected by CNF concentration. The mechanical properties of A-type gelatin films loaded with CNF (0-5%) varied from 45.1±2.5 to 30.7±1.8 MPa for TS; from 19.3±0.1 to 20.3±1.0 for E, and from 11.8±0.5 to 9.2±0.4 MPa for M. B-type gelatin films presented TS varying from 21.8±1.5 to 24.2±1.2 MPa, but with E and M staying around 26% and 6 MPa, respectively. The increase of CNF concentration decreased the mechanical properties of the A-type gelatin films. In contrast, the mechanical properties of B-type gelatin films increased by 41% at 1% CNF concentration compared to the pure film (21.8±1.5-30.8±1.4 MPa); and not evidenced changes at 3% and 5% concentrations. This behavior observed in A-type gelatin films could be attributed to aggregates formed by CNF/gelatin complex coacervates at preparing conditions (pH<pI, 5.30); which acting as break points in the film structure, reducing the mechanical strength. On other hand, the moderate increase observed in B-type gelatin films evidenced a uniform dispersion of the CNF that did not remain to higher CNF concentrations, what could be related to electrostatic repulsive interactions between groups of gelatins (COO−) induced by processing conditions (pH>pI, 6.30), and negatively charged groups of CNF provided by the buffer used in CNF extraction. The mechanical properties of the gelatin films are regulated by CNF concentration and electrostatic interactions CNF/type gelatin defined by the pH.

Share your ideas or questions with the authors!

Did you know that the greatest stimulus in scientific and cultural development is curiosity? Leave your questions or suggestions to the author!

Sign in to interact

Have a question or suggestion? Share your feedback with the authors!

Institutions
  • 1 Department of Food Engineering, Faculty of Animal Science and Food Engineering, University of São Paulo
Track
  • Process engineering and emerging technologies (ET)
Keywords
Nanocellulose
enzymatic hydrolysis
Films