ORGANOSOLV FRACTIONATION OF CORNCOB LIGNIN UNDER GREEN CONDITIONS: A FIRST-ORDER KINETIC APPROACH

Vol.2, 2025 - 334234
Poster
Favorite this paper
How to cite this paper?
Abstract

Corncob, an abundant agro-industrial residue rich in cellulose, hemicellulose, and lignin, requires efficient pretreatment for biorefinery use. The organosolv process (OP) effectively dissolves lignin and enhances enzymatic accessibility. However, conventional OP using high temperatures and inorganic acids as catalysts may degrade cellulose and lignin; citric acid (CA) offers a greener alternative that also stabilize lignin. The present study focused on evaluating the effect of temperature (100, 125, and 150 °C) and reaction time (0, 15, 30, 45, 60, and 120 min) during the OP catalyzed or not by CA (0.5% v/v), conducted in a stainless-steel hydrothermal autoclave reactor. Corncob and extruded corncob were subjected to the organosolv process (OP) under three conditions: extruded corncob + citric acid (CA), extruded corncob alone, and raw corncob + CA. For each condition, 3 g of biomass were treated with 50 mL of 70% v/v ethanol. The process yielded two fractions—solid and liquid. The solid fraction was analyzed for cellulose, hemicellulose, and lignin following U.S. National Renewable Energy Laboratory (NREL) protocols. The liquid fraction was characterized by UV–Vis spectrophotometry at 280 nm to quantify soluble lignin. Lignin defractionation was evaluated by mass balance between the initial and final solid components, and activation energy was calculated using a first-order Arrhenius model (R2 > 0.75). The combined effect of time and temperature promoted lignin solubilization from the solid to the liquid fraction, reaching up to 45% for extruded corncob + CA, 35% for extruded corncob, and 50% for raw corncob. A similar trend was observed for hemicellulose, with solubilization around 40% in the presence of CA and 28% without it. These results correlated with the soluble lignin content quantified in the liquid fraction, reaching up to 8.5% with CA and 7% without. The activation energy, calculated based on lignin fractionation, revealed energy barriers of 5.42 kJ/mol for extruded corncob + CA, 20.54 kJ/mol for extruded corncob, and 23.34 kJ/mol for raw corncob + CA. Kinetics confirmed a synergistic effect between extruded corncob and CA, whereas the non-extruded and acid-free processes exhibited similar activation energies. CA enhanced delignification and has been reported to promote esterification at hydroxyl sites, preventing lignin degradation. Data structure was elucidated through Multiple Factor Analysis, which captured 62.5% of the total variance. The clear segregation of variables by process condition and fraction type (solid/liquid) validated underlying correlations, confirming the potential of these fractionation strategies for circular bioeconomy applications.

Share your ideas or questions with the authors!

Did you know that the greatest stimulus in scientific and cultural development is curiosity? Leave your questions or suggestions to the author!

Sign in to interact

Have a question or suggestion? Share your feedback with the authors!

Institutions
  • 1 Department of Biotechnology, Engineering School of Lorena, Universidade de São Paulo
Track
  • Process Engineering and Emerging Technologies (ET)
Keywords
Organosolv ethanol
Citric acid
Delignification