Favorite this paper
How to cite this paper?
Abstract

This study aimed the production of a ceramic hollow fiber using kaolin membrane by the phase inversion/sintering technique. The composition of the ceramic suspension was 36 wt% of kaolin, 54 wt% of NMP, 0.35 wt% of Arlacel and 9.65 wt% of PESf. This ceramic suspension extruded through a tube-in-orifice spinneret (OD 3 mm, ID 1.2 mm) to a water bath with an air gap of 5 cm and pure water was used as internal and external coagulants. Flows of ceramic suspension and of internal coagulant were controlled at 7 and 15 mL min−1, respectively. The hollow fiber precursor was sintered at 1150°C. Extrusion and sintering conditions resulted in a porous structure, but the phase inversion process did not result in an asymmetric pore size distribution. The water permeability of through the hollow fiber was of 30.99 L/h m² kPa. Due to the morphological characteristics of the produced membrane, it is suggested to be applied as a support for the impregnation of silver nanoparticles. This composite structure presents great potention to be used in sterilization processes.

Share your ideas or questions with the authors!

Did you know that the greatest stimulus in scientific and cultural development is curiosity? Leave your questions or suggestions to the author!

Sign in to interact

Have a question or suggestion? Share your feedback with the authors!

Institutions
  • 1 Universidade Federal de Uberlândia
  • 2 Faculdade de Engenharia Química / Universidade Federal de Uberlândia
  • 3 Universidade Federal de Uberlândia - Faculdade de Engenharia Química
Track
  • 8. Recovery and Purification of Bioproducts
Keywords
Kaolin
hollow fiber
ceramic membrane