Caracterização estrutural e luminescente do luminóforo vermelho SrY2O4:RE3+ (RE3+ = Eu3+, Ce3+) para protótipos de LEDs brancos quentes

Favoritar este trabalho
Como citar esse trabalho?
Detalhes
  • Tipo de apresentação: e-Pôster
  • Eixo temático: Química de Materiais - MAT
  • Palavras chaves: WLEDs; Phosphors; Pechini Synthesis; Red-emitting; solid-state lighting;
  • 1 Faculdade de Ciências e Tecnologia / Universidade Estadual Paulista “Júlio de Mesquita Filho”
  • 2 Instituto de Química / Universidade Estadual Paulista “Júlio de Mesquita Filho”
  • 3 Instituto de Biociências, Letras e Ciências Exatas / Universidade Estadual Paulista “Júlio de Mesquita Filho”
  • 4 Química e Bioquímica / Faculdade de Ciências e Tecnologia / Unesp (Universidade Estadual Paulista)

Caracterização estrutural e luminescente do luminóforo vermelho SrY2O4:RE3+ (RE3+ = Eu3+, Ce3+) para protótipos de LEDs brancos quentes

Leonardo Figueiredo Saraiva

São Paulo State University (UNESP)

Resumo

Nowadays, the main technology within solid-state lighting (SSL) is based on phosphor-converted white light-emitting diodes (PC-WLEDs). However, the mechanism of white light generation produces a bluish-white light dangerous to humans at night considering the regulation of human circadian rhythm1. Therefore, this study introduces the red-emitting Ce3+ (2 at. %), Eu3+ (1, 3, 5 at. %) co-doped SrY2O4 phosphor synthesized by Pechini modified method2, aiming the application in warm WLEDs ideal for night lighting 1. Eu3+ and Ce3+-single and -co-doped samples were synthesized by a precursor resin obtained from metal solution precursors, which was fired at 1100 °C upon CO reducing atmosphere. Both Ce3+-single doped, and Ce3+, Eu3+ co-doped samples were obtained as SrY2O4 single phase whereas SrY2O4:Eu3+ was a mixture of SrY2O4/Y2O3 quantified by Rietveld’s, refinement. The refinement of the Ce3+-doped sample revealed distinct lattice parameters in comparison with the mixture and the disposition of two Y3+ sites in the structure. FTIR also showed the broadening and shifting of the ν(Sr-O) band in the co-doped sample, which suggests the substitution of Sr2+ local sites by Ce3+ and/or Eu3+. However, XPS data showed that there is a proportion of Ce4+ and Ce3+ in the Eu3+ 3% co-doped sample (≈70 % and ≈30 %, respectively), which probably can be taking an important role in the SrY2O4 phase stabilization. Upon 370 nm excitation, the SrY2O4:Ce3+, Eu3+ emission spectrum is a set of broad emission bands within the orange-red spectral region characteristic of Eu3+ while the most intense band was assigned to the one coming from the 5D0 → 7F2 transition. The 5 % Eu3+-doped sample displays the highest emission intensity among the others, implying the insertion of a great quantity of Eu3+ into low-symmetry sites lacking an inversion center. Thus, the phosphor was successfully synthesized as proposed, and Ce3+-doping favors the single-phased system, while the combination of dopants (Eu3+ and Ce3+) yields a red-emitting phosphor upon near-UV excitation. The obtained data suggest the phosphor is a potential candidate for the development of warm WLED prototypes.

Compartilhe suas ideias ou dúvidas com os autores!

Sabia que o maior estímulo no desenvolvimento científico e cultural é a curiosidade? Deixe seus questionamentos ou sugestões para o autor!

Faça login para interagir

Tem uma dúvida ou sugestão? Compartilhe seu feedback com os autores!