Obtenção da alumina anódica nanoporosa a partir da anodização pulsada e a influência dos parâmetros de pulso
Nanoporous Anodic Alumina (NAA) has been obtained by anodization method since last decade. In this period, there was enough research about the influence of the parameters used during the anodization process. Recently different anodization methodologies have been emerged, including the pulse anodization method, which stands out to generate different pore geometries in NAA films by modulating the pulse shape[1] and more organized pores when comparing with the common anodization at certain temperatures[2]. Besides pulse shape, the pulse height and frequency (Figure 1) are parameters that also influence the anodization. As shown in Figure 1, the height is equivalent to potential difference between the maximum and minimum voltage applied. The width of the levels influences on duty cycle that is the fraction of the total period of anodization, which the positive potential is applied, and on the pulse frequency, that is equal to the inverse of the period of each pulse. Figure 2.a shows the SEM image of a NAA sample obtained by pulse method and Figure 2.b represents the diameter distribution obtained by pulse method. The applied parameters influence both morphological and optical properties of the obtained films. The control of pore geometry is directly associated with the pulse format and, consequently, with the refractive index of the sample. In this essay, it is shown different NAA films produced by pulse anodization and their properties.