Resposta elétrica de nanopartículas de Na2Ti3O7 sintetizadas por método sonoquímica
Here, the Sonochemical Method followed by thermal treatment is used to Na2Ti3O7 samples. The nanopowders are characterized by several techniques. The physics properties such as specific surface area, the pore volume, and pore size were determinate, being 51.20 m2/g, 0.070 cm3/g, and 54.69 Å, respectively. Capacitance values for the ceramic sample in the order of μF are obtained. The behavior of total energy of the system was used to determination of the relaxation time of the sample (τ0 = 31 ms). The samples obtained by this method are a good candidate to be used as solid state electrolyte material. An electrical characterization was made to evaluate the electrical response of the material and its possible use as solid state electrolyte material. For this purpose, the discshaped ceramic of 11 mm in diameter and 2.80 mm thick, were sintered at 950 0C for 1 h. The first of them corresponding to the low frequencies is attributed to the grain capacitive behavior. The insert curve corresponds precisely to this region. The capacitance values, for this region, are in the order of μF. The second semicircle formation is associated with the high frequency region. This behavior is related to the most resistive response of grain boundary with increasing frequency