Heteroarquiteturas Obtidas a partir de Óxido de Grafeno, PANI e MnO2: Aplicação em Supercapacitores
The technological progress achieved today demands an increasing energy consumption. In addition, the environmental damages caused by the use of fossil fuels make necessary the development of efficient, renewable and environmentally friendly sources of energy.1 Among the renewable energy sources presented to date, supercapacitor are electrochemical devices that present higher density of power, are environmentally friendly, with high safety and a high cyclical life. The performance of a supercapacitor depends mainly on its electrodes materials and its intrinsic capacitance can be improved by the development of materials with morphology suitable to the kinetics of Faradaic reactions occurring at the electrochemical interface.2 In order to produce supercapacitors of low cost and high capacitive performance, this work aims to study and optimize the synthesis parameters for composites formed by graphene oxide, PANI and MnO2. For the synthesis of the composites, a dispersion of graphene oxide was prepared in basic media. The system was maintained under heating and then acidified with HCl. The α-MnO2 was synthesized hydrothermally from a suspension of graphene oxide containing MnCl2.4H2O using a solution of KMnO4 as oxidizing agent. Parallel to this, a solution of K2S2O8 3 mol L-1 HCl/1 mol L-1 NaCl was prepared. The aniline was then added to the acidic suspension of graphene oxide/ MnO2, which was maintained at 0°C followed by slow addition of the K2S2O8 in order to promote the polymerization. The obtained material was filtered and dried. The electrochemical behavior of the composite and individual components was analyzed by electrochemical measurements. The conventional three-electrode system was used, containing a Pt counter electrode, saturated Ag/AgCl as reference electrode and a Pt disk as working electrode. As electrolyte, Na2SO4 1 mol L-1 solution was used in which the working electrode was polarized in the potential range of 0.0 V to 0.8 V with a scan rate of 10 mV s-1. The results of the structural characterization showed the effective formation of polyaniline on the oxidized matrix of graphene oxide/MnO2. Electrochemical measurements of cyclic voltammetry and chronopotentiometry showed a good capacitive behavior of the composite, with an increase of 80.00 to 846.88 Fg-1 with the addition of 50% by mass of polymer (PAni), which makes it promising for future application in electrodes of supercapacitors of low cost and high performance.