Degradação fotoeletrocatalítica do corante têxtil RB4 sob radiação UV e visível empregando nanotubos de TiO2 modificados com óxidos de cobre
The photocatalytic degradation of textile effluents using nanophotocatalysts through advanced oxidation process is one of the recent scientific explorations that gain importance mainly due to its ability to mineralize a diversity of organic compounds. Among various oxide semiconductor photocatalysts, TiO2 has gained considerable attention because of its outstanding properties including corrosion resistance, chemical stability, no toxicity and photoactivity under UV radiation. It has a band gap energy of 3.2 eV in anatase crystalline phase, equivalent to the absorption wavelength shorter than 388 nm, which corresponds to only UV radiation, making it a major obstacle to its use under sunlight [1]. Copper oxides can be used as an efficient sensitizer to couple with other wide band gap semiconductors, such as TiO2, to expand the photocatalytic application in the visible light area. In this work, TiO2 nanotubes (NT/TiO2) were synthesized on Ti substrate through the anodizing process and decorated by electrodeposition process with copper nanoparticles. After, the samples were annealed at 150 or 300ºC to convert the copper in Cu2O or CuO, respectively. In electrodeposition process was evaluated the influence of electrolyte, lactic acid and Na2SO4, in the distribution and size of the copper nanoparticles, and its photoelectrochemical performance. The electrodes were characterized by SEM-FEG, XRD, XPS, UV-Vis spectroscopy and photocurrents by linear voltammetry experiments in a solution containing 30 ppm of RB4 in 0.1M Na2SO4, pH 3, with a potential range of -0.025 to -1,0 V vs. Ag/AgCl. NT/TiO2-Cu2O and NT/TiO2-CuO electrodes prepared with Na2SO4 and lactic acid were applied as photocatalyst in degradation experiments of the Reactive Blue 4 (RB4) textile dye, under UV and visible light irradiation. Both modified electrodes showed enhanced in the degradation of compounds organics of dyes when compared with NT/TiO2 without copper oxide. However, the NT/TiO2-Cu2O showed better performance in organic load reduction in relation to NT/TiO2-CuO, regardless of the type of electrolyte used. Reduction of the organic load of 91.5% and 79.6% were obtained using NT/TiO2-Cu2O prepared in solution containing lactic acid and Na2SO4, respectively, and only 23.3% for NT/TiO2, under UV radiation and -0.6V vs. Ag/AgCl. Under visible light, TiO2 nanotubes modified with copper oxide exhibited remarkable performance, due to the facility of generation e-/h+ pairs acquired for the system.