Uma nova interpretação para o mecanismo anódico de exfoliação eletroquímica de óxido de grafeno oriundo de pilhas Lechanché exauridas
The present work discuss about the anodic electrochemical exfoliation mechanism (AEEM) of graphene oxide formation from graphite in aqueous systems and its consequences. The electrochemical exfoliation mechanism formation of graphene oxide used a waste source (Leclanché depleted cell) of graphite. The experimental approach it was performed by electrochemical experiments in NaF 1.0 mol L-1 in a condition of non-cavity formation, Raman in 532 nm laser and SEM-FEG. The theoretic approach it was performed by molecular dynamics and semi-empirical calculations. Framed work demonstrated that, there was a surface transformation because of corrosion process by water electrolysis intermediates [1,2]. By Raman spectroscopy, it was observed the nature of chemical structure changes in the electrode surface. These changes it were confirmed by SEM-FEG images, where the influence of oxidation process affects the surface morphology by cracks, valleys, relief and grooves generation. The surface corrosion leads to decreasing in resistance of charge transference and an increase of capacitance values obtained in different exfoliation times. Molecular dynamics (MD) and semi-empirical (SE) simulations it were performed in attempt to clarify the AEEM with 4 models in each methodology. Without the corrosion process, there was not intercalation of electrolytes or water in any potential evaluated in the models studied here. This occurred due to a large energy intercalation barrier (10.13 eV) as showed by semi-empirical simulations. The molecular dynamics showed that hydrophobic surfaces had an intense shielding effect that avoids the electrolytes interacting with the electrode. Hydrophilic surfaces have small shielding effect, which contributes with the intercalation process by electric field action. The SE results shown that the oxidative process on graphitic surfaces were accompanied by structural modifications, such as increasing of interlayer spacing (3,34d to 4,38d) and (110)-sliding between the sheets. Such deformation induces a smaller n-stacking interaction for oxidized models (15,13meV/atom) in comparison to the pristine graphite models (42,31meV/atom). The experimental and theoretical conclusion leads to possibility of graphene oxide exfoliation without cavity formation, a different point of view if compared with literature [3].